C-85 Bauxite

Oxide Analysis Formula Tolerance
CaO 0.10% -
K2O 0.10% -
MgO 0.10% -
Na2O 0.10% -
TiO2 3.52% 0.05
Al2O3 88.44% 1.00
SiO2 6.03% 0.12
Fe2O3 1.60% 0.01
Oxide Weight 115.32
Formula Weight 115.32

Related Information

Links

Typecodes Aluminum Silicate
Materials not classifiable as commonly known aluminum silicates. For example, kaolin is a common aluminum silicate.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy