Barium Oxide-Alumina-Silica Eutectic

Oxide Analysis Formula Tolerance
BaO 35.00% 1.00
Al2O3 10.00% 0.43
SiO2 55.00% 4.01
Oxide Weight 438.00
Formula Weight 438.00

Notes

One person questioned these numbers, citing an alternate source claiming 60% SiO2, 10% Al2O3, 30% BaO.

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1200C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy