1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Inada Kakoogan Pyrophyllite

Oxide Analysis Formula Tolerance
CaO 0.31% 0.02
K2O 0.44% 0.02
MgO 0.14% 0.02
Na2O 0.02% -
TiO2 0.20% 0.01
Al2O3 23.17% 1.00
SiO2 65.56% 4.80
Fe2O3 0.21% 0.01
LOI 9.94%n/a
Oxide Weight 396.42
Formula Weight 440.18