Harris Muscovite

Description: Legacy material

Oxide Analysis Formula Tolerance
K2O 8.93% 0.80
Na2O 1.49% 0.20
Al2O3 34.23% 2.82
P2O5 0.03% -
SiO2 45.65% 6.38
Fe2O3 4.96% 0.26
LOI 4.71%n/a
Oxide Weight 800.47
Formula Weight 840.04