Pemco Frit Pb-113

Alternate Names: Frit Pb113

Description: Very low melting high lead frit

Oxide Analysis Formula Tolerance
PbO 88.10% 1.00
SiO2 11.90% 0.50
Oxide Weight 253.35
Formula Weight 253.35

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.6 x 10-6 (50-450C)
Frit Melting Range (C) 1300-1340F
I.F.P. (celsius) 490C