Ferro Frit CC-270

Notes

A high expansion frit for cone 06-04.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 642
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Available from Laguna Clays

Data

Frit Softening Point 1400F