1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Amakusa Stone

Oxide Analysis Formula Tolerance
CaO 0.05% 0.01
K2O 2.35% 0.15
MgO 0.28% 0.04
TiO2 0.02% -
Al2O3 16.75% 1.00
P2O5 0.01% -
SiO2 77.14% 7.82
Fe2O3 0.42% 0.02
MnO 0.01% -
LOI 2.97%n/a
Oxide Weight 590.87
Formula Weight 608.96

Related Information

Data

Dry M.O.R. (50% Silica) 582C