Description: High magnesia leadless boron-free low expansion frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.50% | 0.01 | |
| MgO | 23.80% | 0.99 | |
| Al2O3 | 26.80% | 0.44 | |
| SiO2 | 48.90% | 1.36 | |
| Oxide Weight | 166.81 | ||
| Formula Weight | 166.81 | ||
Used as a filler in resin bonded abrasives, an MgO source. Very high fire frit with very low expansion at cone 10.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 4.20 |
|---|---|
| Frit Melting Range (C) | 2400F |