Ferro Frit 3247

Description: Leadless very high barium boron free frit

Oxide Analysis Formula Tolerance
BaO 53.10% 1.00
Al2O3 5.30% 0.15
SiO2 41.60% 2.00
Oxide Weight 288.70
Formula Weight 288.70

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Hazards Barium Carbonate in Glazes
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.60
Frit Melting Range (C) 1850F