Super Spar #4

Description: Thai Feldspar

Oxide Analysis Formula Tolerance
SiO2 65.67% 6.34
TiO2 0.01% -
Al2O3 18.89% 1.08
Fe2O3 0.11% -
Na2O 2.55% 0.24
K2O 12.35% 0.76
Oxide Weight 578.17
Formula Weight 578.17

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
URLs http://ceramics.sibelcotools.com/tiles/porcelain-tiles/feldspar/