Frit 33.170

Oxide Analysis Formula Tolerance
CaO 0.96% 0.06
K2O 2.94% 0.11 `
Na2O 13.20% 0.75
MgO 0.92% 0.08
Al2O3 15.06% 0.52
ZrO2 15.04% 0.43
B2O3 7.51% 0.38
SiO2 44.37% 2.60
Oxide Weight 352.05
Formula Weight 352.05

Related Information

Data

Frit Melting Range (C) 1000-1100C