Alternate Names: Frit 37 062, Frit 37-062
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 8.42% | 0.36 | |
| BaO | 29.60% | 0.46 | |
| K2O | 5.73% | 0.15 | |
| MgO | 0.58% | 0.03 | |
| Al2O3 | 5.83% | 0.14 | |
| ZrO2 | 2.64% | 0.05 | |
| B2O3 | 4.23% | 0.15 | |
| SiO2 | 42.97% | 1.71 | |
| Oxide Weight | 239.01 | ||
| Formula Weight | 239.01 | ||
| Frit Melting Range (C) | 980-1060C |
|---|