Frit 37.960

Alternate Names: 37 960,37-960

Oxide Analysis Formula Tolerance
MgO 1.00% 1.00
B2O3 1.09% 0.63
Al2O3 0.32% 0.13
SiO2 1.87% 1.25
Oxide Weight 172.48
Formula Weight 172.48

Related Information

Data

Frit Melting Range (C) 1000-1120C