1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit 35.200

Alternate Names: 35 200, 35-200

Oxide Analysis Formula Tolerance
ZnO 23.50% 0.46
CaO 3.97% 0.11
BaO 12.53% 0.13
MgO 1.54% 0.06
K2O 0.51% 0.01
PbO 21.89% 0.16
Na2O 2.70% 0.07
Al2O3 3.89% 0.06
SiO2 29.47% 0.78
Oxide Weight 159.63
Formula Weight 159.63

Related Information

Data

Frit Melting Range (C) 960-1040C