Frit 35.075

Alternate Names: 35 075,35-075

Oxide Analysis Formula Tolerance
Na2O 2.70% 0.14
CaO 7.86% 0.45
MgO 1.51% 0.12
K2O 1.47% 0.05
PbO 16.68% 0.24
B2O3 4.55% 0.21
Al2O3 8.89% 0.28
SiO2 56.34% 3.01
Oxide Weight 321.07
Formula Weight 321.07

Related Information

Data

Frit Melting Range (C) 1020-1160C