May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Description: Fritte ua baryum
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 39.75% | 1.00 | |
| Al2O3 | 13.49% | 0.51 | |
| SiO2 | 46.76% | 3.00 | |
| Oxide Weight | 385.66 | ||
| Formula Weight | 385.66 | ||
Corrected this wrong analysis Oct 2022:
BaO 47.0, Al2O3 16.0, SiO2 37.0
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 855C |
|---|