Description: Mullite grog
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 58.60% | 1.00 | |
| SiO2 | 37.80% | 1.09 | |
| TiO2 | 2.20% | 0.05 | |
| Fe2O3 | 1.13% | 0.01 | |
| Oxide Weight | 173.59 | ||
| Formula Weight | 173.59 | ||
Other grades are available, see them for more information.
| Materials |
Grog
|
| Materials |
Mulcoa 70 Mullite
|
| Materials |
Mulcoa 47 Calcine Grog
|
| Typecodes |
Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes. |
| Pyrometric Cone Equivalent | 37 |
|---|