May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Alternate Names: Alkalibleiborfritte
Description: Alkaiblei-bortritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 7.15% | 0.25 | |
| PbO | 62.54% | 1.00 | |
| SiO2 | 30.31% | 1.80 | |
| Oxide Weight | 356.89 | ||
| Formula Weight | 356.89 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 117 x 10-7 (20-400C) |
|---|---|
| Heating Microscope Analysis for Frits | 473C |
| Heating Microscope Analysis for Frits | 650C |
| Heating Microscope Analysis for Frits | 800C |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk