Description: A-300 BANGALORE FELDSPAR
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 12.48% | 0.73 | |
| Na2O | 3.01% | 0.27 | |
| Al2O3 | 19.06% | 1.03 | |
| SiO2 | 64.37% | 5.92 | |
| Fe2O3 | 0.19% | 0.01 | |
| LOI | 0.89% | n/a | |
| Oxide Weight | 547.47 | ||
| Formula Weight | 552.39 | ||
Mined and processed in India to sizes down to 800 mesh (4 micron).
Chemical analysis has been supplied by Essen & Co Assayers, Bangalore, India.
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |