Alternate Names: Fritte C1256, Fritte C 1256, Ceradel Frit 1256
Description: Fritte borique, very low expansion borate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 59.00% | 7.07 | |
| Al2O3 | 8.00% | 0.57 | |
| K2O | 0.40% | 0.03 | .75 |
| BaO | 1.50% | 0.07 | 2.5 |
| B2O3 | 24.00% | 2.48 | |
| CaO | 7.00% | 0.90 | |
| Oxide Weight | 719.70 | ||
| Formula Weight | 719.70 | ||
We only have an approximate analysis from the manufacturer. Do you have a precise one?
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Co-efficient of Linear Expansion | 45 (10-7/C 20/300C) |
|---|---|
| Frit Softening Point | 920-1020C M |