Ceradel Frit C 1252

Alternate Names: Fritte C1252, Fritte C 1252, Ceradel Frit 1252

Description: Fritte borocalcique sans plomb

Oxide Analysis Formula Tolerance
B2O3 22.57% 0.98
Al2O3 13.83% 0.41
CaO 15.21% 0.82
Na2O 1.85% 0.09
SiO2 43.73% 2.20
K2O 2.80% 0.09
Oxide Weight 302.37
Formula Weight 302.37

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 58x10-7 (20/300C)
Frit Softening Point 900-980C