Silica Arimao (Cuba)

Description: Cuban silica

Oxide Analysis Formula Tolerance
Al2O3 16.07% 1.16
MgO 1.97% 0.36
CaO 4.90% 0.64
SiO2 67.78% 8.28
Fe2O3 4.69% 0.22
0.48% -
SO4 1.32%n/a
Oxide Weight 700.37
Formula Weight 709.74