Digitalfire is facing a takedown order from Plainsman Clays. They are revoking permission to "use any Plainsman content" "on any platform". This is broad and vague enough, and this site large enough, that I am unable to comply or even interpret it in the short timeframe (June 27). Please don't panic, there are lots of backup sites, don't start downloading or scraping again and overload the server.
Insight-live.com general operation is not affected by this.
Description: Cuban feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 72.57% | 8.47 | |
| Al2O3 | 15.47% | 1.06 | |
| TiO2 | 0.12% | 0.01 | |
| CaO | 1.31% | 0.16 | |
| MgO | 0.69% | 0.12 | |
| K2O | 2.71% | 0.20 | |
| Na2O | 4.55% | 0.51 | |
| Fe2O3 | 0.61% | 0.03 | |
| 1.00% | - | ||
| LOI | 1.25% | n/a | |
| Oxide Weight | 687.31 | ||
| Formula Weight | 696.01 | ||
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| Materials |
Feldspar HolguĂn (Cuba)
|