SPCT #1 Ball Clay

Description: Ball clay for fillers and coating

Notes

A fine-grained engineered blend designed to provide superior viscosity and color (raw and fired) consistency. Ideally suited for a variety of ceramic and non-ceramic filler and coating applications.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy