| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 14.71% | 0.18 | |
| Na2O | 0.39% | 0.01 | |
| CaO | 29.26% | 0.61 | |
| MgO | 5.66% | 0.16 | |
| TiO2 | 0.21% | - | |
| P2O5 | 4.88% | 0.04 | |
| Fe2O3 | 1.26% | 0.01 | |
| Al2O3 | 3.54% | 0.04 | |
| SiO2 | 16.59% | 0.32 | |
| LOI | 0.00% | n/a | |
| Oxide Weight | 89.07 | ||
| Formula Weight | 111.76 | ||