| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 3.68% | 0.41 | |
| K2O | 1.85% | 0.12 | |
| MgO | 1.57% | 0.25 | |
| Na2O | 2.05% | 0.21 | |
| TiO2 | 0.64% | 0.05 | |
| Al2O3 | 13.61% | 0.84 | |
| P2O5 | 0.16% | 0.01 | |
| SiO2 | 65.51% | 6.88 | |
| Fe2O3 | 6.47% | 0.26 | |
| MnO | 0.12% | 0.01 | |
| LOI | 4.35% | n/a | |
| Oxide Weight | 603.97 | ||
| Formula Weight | 631.43 | ||