Opeal OP-5 Ball Clay

Description: Super-white ball clay

Oxide Analysis Formula Tolerance
SiO2 53.12% 2.89
Al2O3 31.20% 1.00
Fe2O3 0.92% 0.02
TiO2 0.54% 0.02
CaO 0.05% -
MgO 0.10% 0.01
K2O 1.21% 0.04
Na2O 0.15% 0.01
LOI 12.80%n/a
Oxide Weight 285.37
Formula Weight 327.26

Notes

Based on OP-4 but improved to meet customers ' demand, low cost of producing, excellent plasticity and excellent whiteness after burning.
Application in high-grade polished tiles, porcelain tiles, sanitary ware, ceramic glaze.

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.
URLs http://www.opeal.com.cn/english/products_op05.htm
OP-5 ball clay information

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy