Description: Super-white ball clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 51.49% | 2.61 | |
| Al2O3 | 33.45% | 1.00 | |
| Fe2O3 | 0.60% | 0.01 | |
| TiO2 | 0.22% | 0.01 | |
| CaO | 0.07% | - | |
| MgO | 0.10% | 0.01 | |
| K2O | 1.17% | 0.04 | |
| Na2O | 0.10% | - | |
| LOI | 12.80% | n/a | |
| Oxide Weight | 265.90 | ||
| Formula Weight | 304.93 | ||
It is not only high in whiteness after 1220C; burning but also excellent in plasticity, reasonable in particle distribution. Application in high-grade polished tiles and tableware.
| URLs |
http://www.opeal.com.cn/english/products_op02.htm
OP-2 ball clay information |
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |