Premium China Clay

Description: Super white burning kaolin

Oxide Analysis Formula Tolerance
TiO2 0.09% -
Al2O3 35.50% 1.00
SiO2 49.50% 2.37
Fe2O3 0.29% 0.01
LOI 13.80%n/a
Oxide Weight 245.32
Formula Weight 284.59