| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.01% | - | |
| MgO | 0.17% | 0.02 | |
| K2O | 10.34% | 0.62 | |
| Na2O | 3.95% | 0.36 | |
| TiO2 | 0.01% | - | |
| Al2O3 | 17.58% | 0.97 | |
| SiO2 | 65.29% | 6.11 | |
| Fe2O3 | 0.07% | - | |
| LOI | 0.36% | n/a | |
| Oxide Weight | 547.69 | ||
| Formula Weight | 549.67 | ||
A New Zealand material.