Formula: CdO
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CdO | 100.00% | 1.00 | |
| Oxide Weight | 128.41 | ||
| Formula Weight | 128.41 | ||
Cadmium oxide is insoluble in water and alkalis, but soluble in acids and ammonium salts.
See notes for CdO oxide for information about participation in glaze chemistry.
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| URLs |
http://en.wikipedia.org/wiki/Cadmium_oxide
Cadmium oxide on Wikipedia |
| Materials |
Stains Encapsulated
|
| Oxides | CdO - Cadmium Oxide |
| Glossary |
Encapsulated Stain
This is a type of stain manufacture that enables the use of metal oxides (like cadmium) under temperature conditions in which they would normally fail. |