Alternate Names: TSP
Description: Anhydrous Trisodium Phosphate
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 56.71% | 0.75 | |
| P2O5 | 43.29% | 0.25 | |
| Oxide Weight | 81.98 | ||
| Formula Weight | 81.98 | ||
| Materials |
Trisodium Phosphate Hydrous
|
| URLs |
http://en.wikipedia.org/wiki/Trisodium_phosphate
Trisodium Phosphate on Wikipedia |
| Oxides | P2O5 - Phosphorus Pentoxide |