Cryolite and Fluorite Eutectic

Oxide Analysis Formula Tolerance
AlF3 29.80% 1.00
NaF 44.80% 3.00
CaF2 25.40% 0.92
Oxide Weight 281.54
Formula Weight 281.54

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 905C