May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 20.00% | 1.00 | |
| Al2O3 | 20.00% | 0.40 | |
| SiO2 | 60.00% | 2.01 | |
| Oxide Weight | 201.50 | ||
| Formula Weight | 201.50 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 1350C |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk