| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 15.60% | 0.71 | |
| CaO | 5.80% | 0.29 | |
| Al2O3 | 36.00% | 0.99 | |
| SiO2 | 42.60% | 2.00 | |
| Oxide Weight | 281.69 | ||
| Formula Weight | 281.69 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 1130C |
|---|