| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 6.80% | 0.59 | |
| K2O | 7.10% | 0.41 | |
| Al2O3 | 19.00% | 1.01 | |
| SiO2 | 67.10% | 6.03 | |
| Oxide Weight | 540.40 | ||
| Formula Weight | 540.40 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 1160C |
|---|