Potash-Silica Eutectic 1

Oxide Analysis Formula Tolerance
K2O 55.00% 1.00
SiO2 45.00% 1.28
Oxide Weight 171.27
Formula Weight 171.27

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 780C