Pemco Frit Pb-2F-35

Alternate Names: Frit Pb-2F35, Frit Pb2F35

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 448
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.