Fusion Frit F-578

Alternate Names: Fusion Frit 578

Description: High barium zero boron frit

Oxide Analysis Formula Tolerance
K2O 3.80% 0.12
Na2O 1.40% 0.07
CaO 5.60% 0.30
BaO 25.50% 0.51
Al2O3 13.00% 0.39
SiO2 50.70% 2.56
Oxide Weight 303.88
Formula Weight 303.88

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.2 x 10-6
Frit Softening Point 1800F