May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Alternate Names: Fusion Frit 435
Description: Boron free high sodium frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 17.00% | 0.71 | |
| K2O | 2.60% | 0.07 | |
| MgO | 1.50% | 0.10 | |
| CaO | 2.80% | 0.13 | |
| SiO2 | 76.10% | 3.26 | |
| Oxide Weight | 257.12 | ||
| Formula Weight | 257.12 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.9 x 10-6 |
|---|---|
| Frit Softening Point | 1650F |