Alternate Names: Fusion Frit F359
Description: Low expansion flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 0.10% | - | |
| CaO | 3.40% | 0.13 | |
| MgO | 16.00% | 0.86 | |
| Al2O3 | 19.50% | 0.42 | |
| SiO2 | 61.00% | 2.21 | |
| Oxide Weight | 217.75 | ||
| Formula Weight | 217.75 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.0 x 10-6 |
|---|---|
| Frit Softening Point | >1900F |