| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.30% | 0.02 | |
| K2O | 0.20% | 0.01 | |
| MgO | 0.30% | 0.03 | |
| Na2O | 0.30% | 0.02 | |
| TiO2 | 1.50% | 0.06 | |
| Al2O3 | 30.10% | 1.00 | |
| SiO2 | 55.30% | 3.12 | |
| Fe2O3 | 1.50% | 0.03 | |
| LOI | 10.50% | n/a | |
| Oxide Weight | 303.29 | ||
| Formula Weight | 338.87 | ||
| Dry M.O.R. (50% Silica) | 851C |
|---|