May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Description: Low alumina very high alkali frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.75% | 0.30 | |
| K2O | 13.01% | 0.30 | |
| Na2O | 11.42% | 0.40 | |
| Al2O3 | 1.41% | 0.03 | |
| SiO2 | 66.41% | 2.40 | |
| Oxide Weight | 217.18 | ||
| Formula Weight | 217.18 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 122.4 x 10-7 C (Appen) |
|---|---|
| Frit Softening Point | 1000-1300C |