MCS

Description: From Ron Roy's MDT

Oxide Analysis Formula Tolerance
CaO 0.31% 0.03
MgO 0.16% 0.02
K2O 1.71% 0.08
Na2O 2.43% 0.18
TiO2 0.47% 0.03
Al2O3 22.32% 1.00
SiO2 66.05% 5.02
Fe2O3 0.55% 0.02
LOI 6.00%n/a
Oxide Weight 429.57
Formula Weight 456.99