1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Lepidolite

Alternate Names: Lithium Mica

Description: From Ron Roys MDT

Oxide Analysis Formula Tolerance
Li2O 4.25% 0.55
K2O 9.57% 0.39
Na2O 1.06% 0.07
Fe2O3 0.13% -
Al2O3 26.65% 1.00
SiO2 58.34% 3.71
Oxide Weight 382.69
Formula Weight 382.69

Related Information

Links

Materials Lepidolite
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.