| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.21% | 0.02 | |
| MgO | 0.12% | 0.01 | |
| K2O | 0.78% | 0.03 | |
| Na2O | 0.20% | 0.01 | |
| TiO2 | 0.84% | 0.04 | |
| Al2O3 | 24.95% | 1.00 | |
| SiO2 | 60.34% | 4.10 | |
| Fe2O3 | 1.42% | 0.04 | |
| MnO | 0.03% | - | |
| LOI | 11.11% | n/a | |
| Oxide Weight | 363.40 | ||
| Formula Weight | 408.82 | ||