FHC

Oxide Analysis Formula Tolerance
Fe2O3 1.61% 0.05
SiO2 66.75% 5.49
Al2O3 20.65% 1.00
TiO2 0.53% 0.03
Na2O 0.55% 0.04
K2O 0.68% 0.04
MgO 0.51% 0.06
CaO 0.50% 0.04
LOI 8.21%n/a
Oxide Weight 453.34
Formula Weight 493.89