Clinchfield #303

Alternate Names: Clinchfield 303

Description: POTASH FELDSPAR

Oxide Analysis Formula Tolerance
CaO 0.50% 0.05
K2O 7.90% 0.46
Na2O 5.50% 0.49
Al2O3 18.20% 0.98
SiO2 67.80% 6.22
Oxide Weight 550.45
Formula Weight 550.45

Notes

Similar to Kingman feldspar.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.