Description: Dankwean Village Sandy Clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 0.55% | 0.07 | |
| MgO | 0.26% | 0.05 | |
| CaO | 0.31% | 0.04 | |
| Fe2O3 | 3.86% | 0.18 | |
| TiO2 | 0.83% | 0.08 | |
| K2O | 0.87% | 0.07 | |
| Al2O3 | 13.83% | 1.00 | |
| SiO2 | 74.53% | 9.15 | |
| LOI | 4.96% | n/a | |
| Oxide Weight | 700.95 | ||
| Formula Weight | 737.53 | ||