Digitalfire will shut down on June 26. I no longer have the authority to grant exemption to a section in the Terms and Conditions of using material in the Insight-Live account from which I built the source material. While there are ways to comply with the take-down order, they are beyond my means because of how complex and large the site has become in the past 35+ years. It has been a wild ride for a shy prairie boy, thanks to everyone for your support. Insight-live.com is not affected by this.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 44.00% | 0.69 | |
| MgO | 43.00% | 1.00 | |
| H2O | 13.00% | n/a | |
| Oxide Weight | 81.54 | ||
| Formula Weight | 93.72 | ||
| Minerals |
Serpentine
A hydrous magnesium iron phyllosilicate mineral. |